Skip to content
Automated comparison · 34% overlap

EN AW-1050A vs EN AW-5083: 34% composition overlap. Significantly different materials serving different application areas.

EN AW-1050A vs EN AW-5083

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-1050A

3.0255

Aluminum1xxx (Pure)

Commercially pure aluminium (99.5% min Al). Excellent corrosion resistance, thermal and electrical conductivity. Very soft and easily formed. Used for chemical plant equipment, food industry, reflectors, heat exchangers, electrical conductors, and decorative trim.

EN AW-5083

3.3547

Aluminum5xxx_mg

The highest-strength non-heat-treatable aluminum alloy. Al-Mg4.5-Mn with outstanding seawater and industrial chemical resistance. Retains exceptional strength after welding (unlike 6xxx/7xxx). ASTM B928 certified for marine service. THE shipbuilding aluminum — also used for rail cars, pressure vessels, cryogenic tanks, truck bodies, and LNG applications. Available O, H111, H116, H321 tempers.

EN AW-1050AEN AW-5083
Material Number3.02553.3547
CategoryAluminumAluminum
StandardEN 573-3EN 485-2

Chemical composition (wt%)

ElementEN AW-1050AEN AW-5083Overlap
Si0–0.25%0–0.4%OK
Mn0–0.05%0.4–1%No overlap
Cr0.05–0.25%
Cu0–0.05%0–0.1%OK

Mechanical properties

PropertyEN AW-1050AEN AW-5083Unit
tensile_strength65–95270–345MPa
yield_strength≥ 20115–130MPa
elongation≥ 23≥ 16%

Compatibility Assessment

EN AW-1050A and EN AW-5083 have significantly different compositions (34% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-1050A the same as EN AW-5083?

EN AW-1050A and EN AW-5083 have a 34% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-1050A with EN AW-5083?

Generally not recommended. The compositions differ significantly (34% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-1050A and EN AW-5083?

The main differences are in the following elements: Mn, Mg. EN AW-1050A is a Aluminum grade, while EN AW-5083 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.