Skip to content
Automated comparison · 9% overlap

14NiCrMo13-4 vs EN-GJL-250: 9% composition overlap. Significantly different materials serving different application areas.

14NiCrMo13-4 vs EN-GJL-250

Side-by-side chemical composition and mechanical property comparison.

Overview

14NiCrMo13-4

1.6657

Alloy SteelCase Hardening

High-nickel case-hardening steel for heavily loaded large gears, shafts, and drivetrain components. Excellent core toughness with case hardness up to 62 HRC after carburizing. The high nickel content (3.0–3.5%) provides superior impact resistance even at low temperatures. Standard material for wind turbine gearboxes, heavy-duty industrial gears, and aerospace transmissions. Also known as EN36C (BS) and similar to SAE 9310.

EN-GJL-250

0.6025

Alloy Steelgrey_cast_iron

Grey cast iron with lamellar graphite and minimum tensile strength 250 MPa. The most widely used grey cast iron grade worldwide. Predominantly pearlitic matrix providing an excellent balance of strength, machinability, damping capacity, and castability. Used for engine blocks, cylinder heads, machine tool beds, lathe beds, flywheels, brake discs, hydraulic valve bodies, and general medium-duty structural castings. Equivalent to DIN GG25 and ASTM A48 Class 35.

14NiCrMo13-4EN-GJL-250
Material Number1.66570.6025
CategoryAlloy SteelAlloy Steel
StandardEN 10084EN 1561

Chemical composition (wt%)

Element14NiCrMo13-4EN-GJL-250Overlap
C0.11–0.17%2.8–3.3%No overlap
Si≤ 0.4%1.2–1.7%No overlap
Mn0.3–0.6%0.8–1.2%No overlap
P≤ 0.025%≤ 0.15%OK

Mechanical properties

Property14NiCrMo13-4EN-GJL-250Unit
tensile_strength1100–1400≥ 250MPa
yield_strength≥ 850MPa
elongation≥ 9%

Compatibility Assessment

14NiCrMo13-4 and EN-GJL-250 have significantly different compositions (9% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is 14NiCrMo13-4 the same as EN-GJL-250?

14NiCrMo13-4 and EN-GJL-250 have a 9% composition overlap. They are generally not directly interchangeable.

Can I replace 14NiCrMo13-4 with EN-GJL-250?

Generally not recommended. The compositions differ significantly (9% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between 14NiCrMo13-4 and EN-GJL-250?

The main differences are in the following elements: C, Si, Mn. 14NiCrMo13-4 is a Alloy Steel grade, while EN-GJL-250 is a Alloy Steel grade.

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.