30NiCrMo16-6 vs EN-GJS-500-7: 26% composition overlap. Significantly different materials serving different application areas.
30NiCrMo16-6 vs EN-GJS-500-7
Side-by-side chemical composition and mechanical property comparison.
Overview
30NiCrMo16-6
1.6747
Ultra-high-strength nickel-chromium-molybdenum steel with outstanding through-hardenability for large cross-sections. Achieves tensile strengths of 1080–1270 MPa (dia ≤40mm) with excellent impact toughness. Very high Jominy hardenability (47–55 HRC). Used for heavy-duty crankshafts, connecting rods, bolts, gear shafts, and critical aerospace structural parts. AFNOR equivalent: 35NCD16.
EN-GJS-500-7
5.3200
Ferritic-pearlitic ductile cast iron with minimum tensile strength 500 MPa and minimum elongation 7%. The balanced grade offering significantly higher strength than EN-GJS-400-15 while retaining reasonable ductility. Mixed ferrite-pearlite matrix (typically 40-50% pearlite). Used for crankshafts, connecting rods, suspension components, gear housings, heavy-duty pipe fittings, and medium-stress structural castings. Equivalent to DIN GGG50, JIS FCD500.
| 30NiCrMo16-6 | EN-GJS-500-7 | |
|---|---|---|
| Material Number | 1.6747 | 5.3200 |
| Category | Alloy Steel | Alloy Steel |
| Standard | EN 10083-3 | EN 1563 |
Chemical composition (wt%)
| Element | 30NiCrMo16-6 | EN-GJS-500-7 | Overlap |
|---|---|---|---|
| C | 0.26–0.33% | 3.2–3.7% | No overlap |
| Si | ≤ 0.4% | 2–2.6% | No overlap |
| Mn | 0.5–0.8% | 0.2–0.5% | Partial |
| P | ≤ 0.025% | ≤ 0.05% | OK |
Mechanical properties
| Property | 30NiCrMo16-6 | EN-GJS-500-7 | Unit |
|---|---|---|---|
| tensile_strength | 1080–1270 | ≥ 500 | MPa |
| yield_strength | ≥ 880 | ≥ 320 | MPa |
| elongation | ≥ 10 | ≥ 7 | % |
Compatibility Assessment
30NiCrMo16-6 and EN-GJS-500-7 have significantly different compositions (26% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is 30NiCrMo16-6 the same as EN-GJS-500-7?
30NiCrMo16-6 and EN-GJS-500-7 have a 26% composition overlap. They are generally not directly interchangeable.
Can I replace 30NiCrMo16-6 with EN-GJS-500-7?
Generally not recommended. The compositions differ significantly (26% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between 30NiCrMo16-6 and EN-GJS-500-7?
The main differences are in the following elements: C, Si, Mn. 30NiCrMo16-6 is a Alloy Steel grade, while EN-GJS-500-7 is a Alloy Steel grade.
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.