Skip to content
Automated comparison · 30% overlap

30NiCrMo16-6 vs EN-GJS-600-3: 30% composition overlap. Significantly different materials serving different application areas.

30NiCrMo16-6 vs EN-GJS-600-3

Side-by-side chemical composition and mechanical property comparison.

Overview

30NiCrMo16-6

1.6747

Alloy SteelQuenched & Tempered

Ultra-high-strength nickel-chromium-molybdenum steel with outstanding through-hardenability for large cross-sections. Achieves tensile strengths of 1080–1270 MPa (dia ≤40mm) with excellent impact toughness. Very high Jominy hardenability (47–55 HRC). Used for heavy-duty crankshafts, connecting rods, bolts, gear shafts, and critical aerospace structural parts. AFNOR equivalent: 35NCD16.

EN-GJS-600-3

5.3201

Alloy Steelductile_cast_iron

Mainly pearlitic ductile cast iron with minimum tensile strength 600 MPa and minimum elongation 3%. High-strength grade achieved through predominantly pearlitic matrix, often with Cu or Sn additions as pearlite stabilizers. Used for camshafts, gears, high-stress housings, heavy-duty hydraulic components, press frames, and load-bearing structural castings where high strength is more important than ductility. Equivalent to DIN GGG60, JIS FCD600.

30NiCrMo16-6EN-GJS-600-3
Material Number1.67475.3201
CategoryAlloy SteelAlloy Steel
StandardEN 10083-3EN 1563

Chemical composition (wt%)

Element30NiCrMo16-6EN-GJS-600-3Overlap
C0.26–0.33%3–3.6%No overlap
Si≤ 0.4%2–2.6%No overlap
Mn0.5–0.8%0.3–0.6%Partial
P≤ 0.025%≤ 0.05%OK

Mechanical properties

Property30NiCrMo16-6EN-GJS-600-3Unit
tensile_strength1080–1270≥ 600MPa
yield_strength≥ 880≥ 370MPa
elongation≥ 10≥ 3%

Compatibility Assessment

30NiCrMo16-6 and EN-GJS-600-3 have significantly different compositions (30% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is 30NiCrMo16-6 the same as EN-GJS-600-3?

30NiCrMo16-6 and EN-GJS-600-3 have a 30% composition overlap. They are generally not directly interchangeable.

Can I replace 30NiCrMo16-6 with EN-GJS-600-3?

Generally not recommended. The compositions differ significantly (30% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between 30NiCrMo16-6 and EN-GJS-600-3?

The main differences are in the following elements: C, Si, Mn. 30NiCrMo16-6 is a Alloy Steel grade, while EN-GJS-600-3 is a Alloy Steel grade.

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.