EN AW-5083 vs EN AW-5052: 49% composition overlap. Significantly different materials serving different application areas.
EN AW-5083 vs EN AW-5052
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-5083
3.3547
The highest-strength non-heat-treatable aluminium alloy. Excellent corrosion resistance (especially seawater), good weldability. Standard alloy for shipbuilding, offshore, pressure vessels, cryogenic applications, and armour plate. Not for continuous service above 65°C under stress (SCC risk).
EN AW-5052
EN AW-5052
General-purpose Al-Mg alloy — Mg 2.2-2.8%. Good balance of formability, corrosion resistance, and moderate strength (UTS 210-260 H32). Non-heat-treatable — strengthened by cold work. THE most widely used 5xxx alloy globally by tonnage. Used for sheet metal work, fuel tanks, marine components, appliances, lighting, and general fabrication. Excellent weldability.
| EN AW-5083 | EN AW-5052 | |
|---|---|---|
| Material Number | 3.3547 | EN AW-5052 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | EN 573-3 |
Chemical composition (wt%)
| Element | EN AW-5083 | EN AW-5052 | Overlap |
|---|---|---|---|
| Si | 0–0.4% | 0–0.25% | OK |
| Mn | 0.4–1% | — | — |
| Cr | 0.05–0.25% | 0.15–0.35% | Partial |
| Cu | 0–0.1% | — | — |
Mechanical properties
| Property | EN AW-5083 | EN AW-5052 | Unit |
|---|---|---|---|
| tensile_strength | 275–350 | 210–260 | MPa |
| yield_strength | ≥ 125 | 160–210 | MPa |
| elongation | ≥ 12 | 7–12 | % |
Compatibility Assessment
EN AW-5083 and EN AW-5052 have significantly different compositions (49% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-5083 the same as EN AW-5052?
EN AW-5083 and EN AW-5052 have a 49% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-5083 with EN AW-5052?
Generally not recommended. The compositions differ significantly (49% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-5083 and EN AW-5052?
The main differences are in the following elements: Cr, Mg. EN AW-5083 is a Aluminum grade, while EN AW-5052 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.