EN AW-5083

3.3547

Aluminum5xxx (Al-Mg)

The highest-strength non-heat-treatable aluminium alloy. Excellent corrosion resistance (especially seawater), good weldability. Standard alloy for shipbuilding, offshore, pressure vessels, cryogenic applications, and armour plate. Not for continuous service above 65°C under stress (SCC risk).

EN AW-6082

3.2315

Aluminum6xxx_mg_si

THE European structural aluminum alloy — AlSi1MgMn. Highest strength in the 6xxx series (UTS 310 T6). Excellent machinability, good weldability (but HAZ softening), and good corrosion resistance. THE default choice for structural aluminum in Europe — equivalent to what 6061 is in the US. Used for bridges, cranes, transport structures, offshore, and machined components.

EN AW-5083EN AW-6082
Material Number3.35473.2315
CategoryAluminumAluminum
StandardEN 573-3EN 755-2

Chemical composition (wt%)

ElementEN AW-5083EN AW-6082Overlap
Si0–0.4%0.7–1.3%No overlap
Mn0.4–1%0.4–1%OK
Cr0.05–0.25%0–0.25%OK
Cu0–0.1%0–0.1%OK

Mechanical properties

PropertyEN AW-5083EN AW-6082Unit
tensile_strength275–350290–340MPa
yield_strength≥ 125250–290MPa
elongation≥ 128–10%

Compatibility Assessment

EN AW-5083 and EN AW-6082 have moderate differences (63% overlap). They are generally not direct substitutes. Consider the specific requirements of your application.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-5083 the same as EN AW-6082?

EN AW-5083 and EN AW-6082 have a 63% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-5083 with EN AW-6082?

Generally not recommended. The compositions differ significantly (63% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-5083 and EN AW-6082?

The main differences are in the following elements: Si, Mg. EN AW-5083 is a Aluminum grade, while EN AW-6082 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.