EN AW-5182 vs EN AW-3004: 43% composition overlap. Significantly different materials serving different application areas.
EN AW-5182 vs EN AW-3004
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-5182
3.3519
One of the strongest non-heat-treatable Al-Mg alloys. 4.5% Mg + 0.35% Mn. THE standard alloy for beverage can lids/pull tabs (H48 temper). Also used for automotive body panels (hoods, doors), fuel tanks, and marine components. Excellent corrosion resistance and formability.
EN AW-3004
EN AW-3004
Al-Mn-Mg alloy — THE beverage can body material. Mn 1.0-1.5% + Mg 0.8-1.3% give moderate strength (UTS 240-280 H19) with excellent formability for deep drawing and ironing. ~200 billion cans/year worldwide. Also used for roofing sheet, color-coated panels, and storage tanks. Stronger than 3003 due to Mg addition.
| EN AW-5182 | EN AW-3004 | |
|---|---|---|
| Material Number | 3.3519 | EN AW-3004 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | EN 573-3 |
Chemical composition (wt%)
| Element | EN AW-5182 | EN AW-3004 | Overlap |
|---|---|---|---|
| Si | 0–0.2% | 0–0.3% | OK |
| Mn | 0.2–0.5% | 1–1.5% | No overlap |
| Cr | 0–0.1% | — | — |
| Cu | 0–0.15% | — | — |
Mechanical properties
| Property | EN AW-5182 | EN AW-3004 | Unit |
|---|---|---|---|
| tensile_strength | 275–330 | 230–270 | MPa |
| yield_strength | 130–190 | 190–230 | MPa |
| elongation | 20–25 | 5–9 | % |
Compatibility Assessment
EN AW-5182 and EN AW-3004 have significantly different compositions (43% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-5182 the same as EN AW-3004?
EN AW-5182 and EN AW-3004 have a 43% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-5182 with EN AW-3004?
Generally not recommended. The compositions differ significantly (43% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-5182 and EN AW-3004?
The main differences are in the following elements: Mn, Mg. EN AW-5182 is a Aluminum grade, while EN AW-3004 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.