Skip to content
Automated comparison · 49% overlap

EN AW-5182 vs EN AW-5356: 49% composition overlap. Significantly different materials serving different application areas.

EN AW-5182 vs EN AW-5356

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-5182

3.3519

Aluminum5xxx_mg

One of the strongest non-heat-treatable Al-Mg alloys. 4.5% Mg + 0.35% Mn. THE standard alloy for beverage can lids/pull tabs (H48 temper). Also used for automotive body panels (hoods, doors), fuel tanks, and marine components. Excellent corrosion resistance and formability.

EN AW-5356

EN AW-5356

Aluminum5xxx_al_mg

THE magnesium-aluminum welding filler wire — Mg 4.5-5.5% + Cr 0.05-0.20%. Together with 4043, accounts for the vast majority of all Al welding wire sold. ER5356/AlMg5Cr(A). Better color match after anodizing than 4043 (no dark spots). Higher weld strength than 4043. Used for MIG/TIG welding of 5xxx and 6xxx base alloys. THE filler for marine, structural, and anodized applications.

EN AW-5182EN AW-5356
Material Number3.3519EN AW-5356
CategoryAluminumAluminum
StandardEN 573-3AWS A5.10

Chemical composition (wt%)

ElementEN AW-5182EN AW-5356Overlap
Si0–0.2%0–0.25%OK
Mn0.2–0.5%0.05–0.2%Partial
Cr0–0.1%0.05–0.2%Partial
Cu0–0.15%

Mechanical properties

PropertyEN AW-5182EN AW-5356Unit
tensile_strength275–330245–285MPa
yield_strength130–190120–165MPa
elongation20–2517–25%

Compatibility Assessment

EN AW-5182 and EN AW-5356 have significantly different compositions (49% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-5182 the same as EN AW-5356?

EN AW-5182 and EN AW-5356 have a 49% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-5182 with EN AW-5356?

Generally not recommended. The compositions differ significantly (49% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-5182 and EN AW-5356?

The main differences are in the following elements: Mn, Cr, Ti, Mg. EN AW-5182 is a Aluminum grade, while EN AW-5356 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.