EN AW-6063 vs EN AC-AlSi10Mg: 34% composition overlap. Significantly different materials serving different application areas.
EN AW-6063 vs EN AC-AlSi10Mg
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-6063
3.3206
The most common extrusion alloy worldwide. Excellent surface finish, good corrosion resistance, and exceptional extrudability. The standard choice for architectural profiles (window frames, curtain walls, railings), heat sinks, and electrical enclosures.
EN AC-AlSi10Mg
EN AC-43000
Versatile aluminum casting alloy with excellent castability and good mechanical properties. THE standard alloy for metal 3D printing (SLM/DMLS/L-PBF) due to its excellent processability with laser powder bed fusion. Also widely used in conventional sand casting and gravity die casting. Si 9-11% provides outstanding fluidity and low shrinkage. Used for automotive structural parts, aerospace components, 3D-printed functional prototypes and series parts, heat exchangers, and complex thin-walled castings.
| EN AW-6063 | EN AC-AlSi10Mg | |
|---|---|---|
| Material Number | 3.3206 | EN AC-43000 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | EN 1706 |
Chemical composition (wt%)
| Element | EN AW-6063 | EN AC-AlSi10Mg | Overlap |
|---|---|---|---|
| Si | 0.2–0.6% | 9–11% | No overlap |
| Mn | 0–0.1% | ≤ 0.45% | OK |
| Cr | 0–0.1% | — | — |
| Cu | 0–0.1% | ≤ 0.05% | OK |
Mechanical properties
| Property | EN AW-6063 | EN AC-AlSi10Mg | Unit |
|---|---|---|---|
| tensile_strength | ≥ 215 | ≥ 150 | MPa |
| yield_strength | ≥ 170 | ≥ 80 | MPa |
| elongation | ≥ 8 | ≥ 2 | % |
Compatibility Assessment
EN AW-6063 and EN AC-AlSi10Mg have significantly different compositions (34% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-6063 the same as EN AC-AlSi10Mg?
EN AW-6063 and EN AC-AlSi10Mg have a 34% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-6063 with EN AC-AlSi10Mg?
Generally not recommended. The compositions differ significantly (34% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-6063 and EN AC-AlSi10Mg?
The main differences are in the following elements: Si, Mg. EN AW-6063 is a Aluminum grade, while EN AC-AlSi10Mg is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.