EN AW-6063 vs EN AW-2011

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-6063

3.3206

Aluminum6xxx (Al-Mg-Si)

The most common extrusion alloy worldwide. Excellent surface finish, good corrosion resistance, and exceptional extrudability. The standard choice for architectural profiles (window frames, curtain walls, railings), heat sinks, and electrical enclosures.

EN AW-2011

3.1655

Aluminum2xxx_cu

The original free-cutting aluminum alloy. Al-Cu with Pb+Bi additions for chip-breaking — the highest machinability rating of any Al alloy. Being phased out in EU for RoHS compliance (Pb content). Replaced by 6026 (Bi only) or 6082 in new designs. Still widely used in US/Asia. Used for high-volume screw machine products, precision bushings, fittings, and instruments.

EN AW-6063EN AW-2011
Material Number3.32063.1655
CategoryAluminumAluminum
StandardEN 573-3EN 573-3

Chemical composition (wt%)

ElementEN AW-6063EN AW-2011Overlap
Si0.2–0.6%0–0.4%Partial
Mn0–0.1%
Cr0–0.1%
Cu0–0.1%5–6%No overlap

Mechanical properties

PropertyEN AW-6063EN AW-2011Unit
tensile_strength≥ 215365–395MPa
yield_strength≥ 170290–310MPa
elongation≥ 88–12%

Compatibility Assessment

EN AW-6063 and EN AW-2011 have significantly different compositions (29% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-6063 the same as EN AW-2011?

EN AW-6063 and EN AW-2011 have a 29% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-6063 with EN AW-2011?

Generally not recommended. The compositions differ significantly (29% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-6063 and EN AW-2011?

The main differences are in the following elements: Si, Cu. EN AW-6063 is a Aluminum grade, while EN AW-2011 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.