Skip to content
Automated comparison · 27% overlap

EN AW-6082 vs EN AW-5356: 27% composition overlap. Significantly different materials serving different application areas.

EN AW-6082 vs EN AW-5356

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-6082

3.2315

Aluminum6xxx (Al-Mg-Si)

High-strength structural aluminium alloy in the Al-Mg-Si family. One of the strongest 6xxx series alloys due to manganese addition. Replaced 6061 in many European applications. Used for trusses, bridges, cranes, transport, scaffolding, and marine applications. Heat treatable (T6/T651).

EN AW-5356

EN AW-5356

Aluminum5xxx_al_mg

THE magnesium-aluminum welding filler wire — Mg 4.5-5.5% + Cr 0.05-0.20%. Together with 4043, accounts for the vast majority of all Al welding wire sold. ER5356/AlMg5Cr(A). Better color match after anodizing than 4043 (no dark spots). Higher weld strength than 4043. Used for MIG/TIG welding of 5xxx and 6xxx base alloys. THE filler for marine, structural, and anodized applications.

EN AW-6082EN AW-5356
Material Number3.2315EN AW-5356
CategoryAluminumAluminum
StandardEN 573-3AWS A5.10

Chemical composition (wt%)

ElementEN AW-6082EN AW-5356Overlap
Si0.7–1.3%0–0.25%No overlap
Mn0.4–1%0.05–0.2%No overlap
Cr0–0.25%0.05–0.2%OK
Cu0–0.1%

Mechanical properties

PropertyEN AW-6082EN AW-5356Unit
tensile_strength≥ 310245–285MPa
yield_strength≥ 260120–165MPa
elongation≥ 817–25%

Compatibility Assessment

EN AW-6082 and EN AW-5356 have significantly different compositions (27% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-6082 the same as EN AW-5356?

EN AW-6082 and EN AW-5356 have a 27% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-6082 with EN AW-5356?

Generally not recommended. The compositions differ significantly (27% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-6082 and EN AW-5356?

The main differences are in the following elements: Si, Mn, Ti, Mg. EN AW-6082 is a Aluminum grade, while EN AW-5356 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.