EN AW-7050 vs EN AC-AlSi7Mg0.3: 34% composition overlap. Significantly different materials serving different application areas.
EN AW-7050 vs EN AC-AlSi7Mg0.3
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-7050
3.4144
High-strength aerospace aluminium developed by Alcoa for thick-plate applications. Zr addition (instead of Cr) reduces quench sensitivity for superior properties in thick sections. T7451 temper gives excellent SCC resistance + fracture toughness. Used for fuselage frames, bulkheads, wing spars, and thick structural aerospace components.
EN AC-AlSi7Mg0.3
EN AC-42100
The most important aluminum sand and gravity die casting alloy worldwide. Excellent castability, good mechanical properties after T6 heat treatment, and outstanding weldability. Si 6.5-7.5% provides excellent fluidity, Mg 0.25-0.45% enables precipitation hardening. Used for automotive wheels, suspension components, aerospace structural castings, engine brackets, and high-integrity safety-critical castings. Equivalent to ASTM A356.0 and DIN G-AlSi7Mg.
| EN AW-7050 | EN AC-AlSi7Mg0.3 | |
|---|---|---|
| Material Number | 3.4144 | EN AC-42100 |
| Category | Aluminum | Aluminum |
| Standard | AMS 4050 | EN 1706 |
Chemical composition (wt%)
| Element | EN AW-7050 | EN AC-AlSi7Mg0.3 | Overlap |
|---|---|---|---|
| Si | 0–0.12% | 6.5–7.5% | No overlap |
| Mn | 0–0.1% | ≤ 0.1% | OK |
| Cu | 2–2.6% | ≤ 0.05% | No overlap |
| Ti | 0–0.06% | ≤ 0.25% | OK |
Mechanical properties
| Property | EN AW-7050 | EN AC-AlSi7Mg0.3 | Unit |
|---|---|---|---|
| tensile_strength | ≥ 510 | ≥ 140 | MPa |
| yield_strength | ≥ 450 | ≥ 80 | MPa |
| elongation | ≥ 9 | ≥ 2 | % |
Compatibility Assessment
EN AW-7050 and EN AC-AlSi7Mg0.3 have significantly different compositions (34% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-7050 the same as EN AC-AlSi7Mg0.3?
EN AW-7050 and EN AC-AlSi7Mg0.3 have a 34% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-7050 with EN AC-AlSi7Mg0.3?
Generally not recommended. The compositions differ significantly (34% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-7050 and EN AC-AlSi7Mg0.3?
The main differences are in the following elements: Si, Cu, Mg. EN AW-7050 is a Aluminum grade, while EN AC-AlSi7Mg0.3 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.