C22E vs S690Q: 40% composition overlap. Significantly different materials serving different application areas.
C22E vs S690Q
Side-by-side chemical composition and mechanical property comparison.
Overview
C22E
1.1151
Low-carbon unalloyed steel for case hardening and general engineering — 0.17-0.24% C. After carburizing: surface HRC 55-60, soft tough core. Much cheaper than alloy case-hardening steels (16MnCr5, 20MnCr5). Modern designation for Ck22. Used for pins, bolts, levers, lightly loaded gears, and any carburized part where alloy additions are not justified. Also used as cold-heading wire.
S690Q
1.8928
High-strength quenched and tempered structural steel — YS 690 MPa min. Part of EN 10025-6 series (S500Q to S960Q). Good weldability despite high strength (CEV controlled). Used for mobile cranes, mining equipment, truck chassis, bridge components, and any structure where weight reduction through higher strength is critical. "Q" = quenched, "L" variants add low-temp impact.
| C22E | S690Q | |
|---|---|---|
| Material Number | 1.1151 | 1.8928 |
| Category | Carbon Steel | Carbon Steel |
| Standard | EN 10083-2 | EN 10025-6 |
Chemical composition (wt%)
| Element | C22E | S690Q | Overlap |
|---|---|---|---|
| C | 0.17–0.24% | 0–0.2% | Partial |
| Si | 0–0.4% | 0–0.8% | OK |
| Mn | 0.4–0.7% | 0–1.7% | OK |
| P | 0–0.025% | 0–0.02% | OK |
Mechanical properties
| Property | C22E | S690Q | Unit |
|---|---|---|---|
| tensile_strength | 410–540 | 770–940 | MPa |
| yield_strength | 240–280 | ≥ 690 | MPa |
| elongation | 22–28 | ≥ 14 | % |
Compatibility Assessment
C22E and S690Q have significantly different compositions (40% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is C22E the same as S690Q?
C22E and S690Q have a 40% composition overlap. They are generally not directly interchangeable.
Can I replace C22E with S690Q?
Generally not recommended. The compositions differ significantly (40% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between C22E and S690Q?
The main differences are in the following elements: C. C22E is a Carbon Steel grade, while S690Q is a Carbon Steel grade.
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.