EN AC-AlSi9Cu3(Fe) vs EN AW-6005A: 35% composition overlap. Significantly different materials serving different application areas.
EN AC-AlSi9Cu3(Fe) vs EN AW-6005A
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AC-AlSi9Cu3(Fe)
EN AC-46000
The most widely used aluminum high-pressure die casting alloy in Europe. Si 8-11% and Cu 2-4% provide excellent castability and good strength without heat treatment. Higher Fe tolerance (up to 1.3%) prevents die soldering in HPDC. NOT heat-treatable (Cu and Fe form insoluble phases). Used for engine blocks, transmission housings, structural automotive die castings, power tool housings, and industrial die cast components. Equivalent to ASTM A380.0.
EN AW-6005A
EN AW-6005A
Al-Mg-Si extrusion alloy β between 6063 (softer) and 6082 (stronger) in the strength range. Optimized for medium-strength extruded profiles with good surface finish. T6: UTS 260-310 MPa. THE European rail vehicle and bus body profile alloy. Also used for structural profiles (curtain walls, ladders, scaffolding), heat sinks, and general engineering extrusions.
| EN AC-AlSi9Cu3(Fe) | EN AW-6005A | |
|---|---|---|
| Material Number | EN AC-46000 | EN AW-6005A |
| Category | Aluminum | Aluminum |
| Standard | EN 1706 | EN 573-3 |
Chemical composition (wt%) β Pro
| Element | EN AC-AlSi9Cu3(Fe) | EN AW-6005A | Overlap |
|---|---|---|---|
| Si | 8β11% | 0.5β0.9% | No overlap |
| Mn | β€ 0.55% | 0β0.5% | OK |
| Cr | β | 0β0.3% | β |
| Cu | 2β4% | β | β |
| Al | |||
| Ti | |||
| Fe | |||
| Mg | |||
| Zn |
Sign up free and get 3 full comparisons immediately.
Sign up free β 3 comparisons/day freeMechanical properties β Pro
| Property | EN AC-AlSi9Cu3(Fe) | EN AW-6005A | Unit |
|---|---|---|---|
| Tensile Strength | β₯ 240 | 260β310 | MPa |
| Yield Strength | β₯ 140 | 215β260 | MPa |
| Elongation | β₯ 1 | 8β12 | % |
| Hardness HB | |||
| Density | |||
| Elastic Modulus |
Sign up free and get 3 full comparisons immediately.
Sign up free β 3 comparisons/day freeCompatibility Assessment
EN AC-AlSi9Cu3(Fe) and EN AW-6005A have significantly different compositions (35% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AC-AlSi9Cu3(Fe) the same as EN AW-6005A?
EN AC-AlSi9Cu3(Fe) and EN AW-6005A have a 35% composition overlap. They are generally not directly interchangeable.
Can I replace EN AC-AlSi9Cu3(Fe) with EN AW-6005A?
Generally not recommended. The compositions differ significantly (35% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AC-AlSi9Cu3(Fe) and EN AW-6005A?
The main differences are in the following elements: Si, Mg. EN AC-AlSi9Cu3(Fe) is a Aluminum grade, while EN AW-6005A is a Aluminum grade.
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.