Skip to content
Automated comparison · 30% overlap

EN-GJS-600-3 vs S355J2W: 30% composition overlap. Significantly different materials serving different application areas.

EN-GJS-600-3 vs S355J2W

Side-by-side chemical composition and mechanical property comparison.

Overview

EN-GJS-600-3

5.3201

Alloy Steelductile_cast_iron

Mainly pearlitic ductile cast iron with minimum tensile strength 600 MPa and minimum elongation 3%. High-strength grade achieved through predominantly pearlitic matrix, often with Cu or Sn additions as pearlite stabilizers. Used for camshafts, gears, high-stress housings, heavy-duty hydraulic components, press frames, and load-bearing structural castings where high strength is more important than ductility. Equivalent to DIN GGG60, JIS FCD600.

S355J2W

1.8965

Alloy SteelWeathering

The most widely used structural weathering steel with minimum yield strength 355 MPa and impact testing at -20°C (J2 designation). Forms a protective patina of stable rust that eliminates the need for painting. Cu, Cr, and P additions provide atmospheric corrosion resistance up to 8 times that of plain carbon steel. Used for unpainted bridges, outdoor sculptures, railway wagons, architectural facades, transmission towers, and containers. Equivalent to ASTM A588 / Corten B.

EN-GJS-600-3S355J2W
Material Number5.32011.8965
CategoryAlloy SteelAlloy Steel
StandardEN 1563EN 10025-5

Chemical composition (wt%)

ElementEN-GJS-600-3S355J2WOverlap
C3–3.6%≤ 0.16%No overlap
Si2–2.6%≤ 0.5%No overlap
Mn0.3–0.6%0.5–1.5%Partial
P≤ 0.05%≤ 0.03%OK

Mechanical properties

PropertyEN-GJS-600-3S355J2WUnit
tensile_strength≥ 600470–630MPa
yield_strength≥ 370≥ 355MPa
elongation≥ 3≥ 20%

Compatibility Assessment

EN-GJS-600-3 and S355J2W have significantly different compositions (30% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN-GJS-600-3 the same as S355J2W?

EN-GJS-600-3 and S355J2W have a 30% composition overlap. They are generally not directly interchangeable.

Can I replace EN-GJS-600-3 with S355J2W?

Generally not recommended. The compositions differ significantly (30% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN-GJS-600-3 and S355J2W?

The main differences are in the following elements: C, Si, Mn, Cu. EN-GJS-600-3 is a Alloy Steel grade, while S355J2W is a Alloy Steel grade.

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.