FKM (Fluoroelastomer / Viton) vs PC/ABS (Blend): 0% composition overlap. Significantly different materials serving different application areas.
FKM (Fluoroelastomer / Viton) vs PC/ABS (Blend)
Side-by-side chemical composition and mechanical property comparison.
Overview
FKM (Fluoroelastomer / Viton)
Fluoroelastomer — THE high-temperature and chemical-resistant rubber. Outstanding resistance to oils, fuels, acids, and solvents at temperatures up to 200°C (short-term 230°C). Fluorine content (64-70%) determines chemical resistance. Trade names: Viton (Chemours), Tecnoflon (Solvay), Dai-El (Daikin). 5-10x more expensive than NBR. Used for aerospace fuel seals, chemical process seals, automotive fuel injector O-rings, semiconductor processing, and any seal exposed to aggressive chemicals at high temperature.
PC/ABS (Blend)
Polycarbonate + ABS blend — one of the most widely used industrial thermoplastic alloys. Combines PC impact strength and heat resistance with ABS processability and lower cost. Better chemical resistance than pure PC. Properties tunable by PC/ABS ratio. Trade names include Bayblend (Covestro), Cycoloy (SABIC), Pulse (Techpolymers). Used for automotive dashboards, laptop/phone housings, power tool casings, and 3D printing (FDM filament).
| FKM (Fluoroelastomer / Viton) | PC/ABS (Blend) | |
|---|---|---|
| Material Number | — | — |
| Category | Polymers | Polymers |
| Standard | ISO 37 | ISO 10350 |
Mechanical properties
| Property | FKM (Fluoroelastomer / Viton) | PC/ABS (Blend) | Unit |
|---|---|---|---|
| tensile_strength | 8–17 | 45–60 | MPa |
| elongation | 150–350 | 50–120 | % |
| hardness_shore_a | 60–90 | — | Shore A |
Compatibility Assessment
FKM (Fluoroelastomer / Viton) and PC/ABS (Blend) have significantly different compositions (0% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is FKM (Fluoroelastomer / Viton) the same as PC/ABS (Blend)?
FKM (Fluoroelastomer / Viton) and PC/ABS (Blend) have a 0% composition overlap. They are generally not directly interchangeable.
Can I replace FKM (Fluoroelastomer / Viton) with PC/ABS (Blend)?
Generally not recommended. The compositions differ significantly (0% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between FKM (Fluoroelastomer / Viton) and PC/ABS (Blend)?
The main differences are in the following elements: overall alloying content. FKM (Fluoroelastomer / Viton) is a Polymers grade, while PC/ABS (Blend) is a Polymers grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.