Skip to content

316LN / X2CrNiMoN17-13-3

1.4429
stainlessaustenitic
Export PDF€4.90

Nitrogen-enhanced low-carbon version of 316. The N addition (0.12-0.22%) increases yield strength by ~30% over 316L without losing corrosion resistance or weldability. Used for pressure vessels, nuclear components, and structural applications requiring higher design stress.

International equivalents

FlagStandardCountryGradeNumberMatch
🇺🇸AISIUSAAISI 316LNS31653REF
🇪🇺ENEuropeX2CrNiMoN17-13-31.4429100%
🇯🇵JISJapanSUS316LN98%

Sources: ASTM A240, EN 10088-2, JIS G4303

Mechanical properties

Compatibility verdict

316LN / X2CrNiMoN17-13-3 and SUS316LN: 98% composition match

Related materials

More Stainless materials →

Export this comparison as PDF

Professional datasheet with equivalents, composition, and properties. Ready for your QM documentation.

Download PDF — €4.90