Skip to content

Alloy 800H / Incoloy 800H

1.4958
Nickel Alloysfe_ni_cr
Compare with…Export PDF

Iron-nickel-chromium alloy (Fe-32Ni-21Cr) with controlled carbon (0.05–0.10%) and grain size for optimized creep-rupture strength above 600°C. Solution-annealed: Rm ≥450 MPa, Rp0.2 ≥170 MPa, A ≥30%. Density 7.94 g/cm³, E-Modul 196 GPa. Excellent resistance to carburization, oxidation, and nitriding to 1100°C. UNS N08810, ASTM B407/B408/B409. Applications: ethylene cracking tubes, reformer furnace tubes, heat exchangers, nuclear steam generators, chemical reactors. Variant 800HT (N08811/1.4959) has tighter Al+Ti control for even higher creep strength.

International equivalents

FlagStandardCountryGradeNumberMatch
🇺🇸UNSUSAN08810—%
🇪🇺ENEuropeX5NiCrAlTi31-201.4958%
🇺🇸ASTMUSAB407/B408/B409—%
🇺🇸Special MetalsUSAIncoloy 800H—%
🇩🇪VDMGermanyNicrofer 3220 H—%
🇸🇪AlleimaSwedenSanicro 31H—%

Sources: SAE/ASTM, EN 10302, ASTM, specialmetals.com, vdm-metals.com, alleima.com

Chemical composition comparison (wt%)

Side-by-side: Alloy 800H / Incoloy 800H (TYPICAL) (VDM Metals / Special Metals) vs N08810 (UNS)

ElementAlloy 800H / Incoloy 800H (TYPICAL)N08810 (UNS)Overlap
C0.05–0.1%——
Si≤ 1%——
Mn≤ 1.5%——
Cr19–23%——
Ni30–35%——
Cu≤ 0.75%——
Al0.25–0.6%——
Ti0.25–0.6%——
Fe≥ 39.5%——

Mechanical properties

Solution-Annealed

PropertyValueUnit
Density≥ 7.94g/cm3
Tensile Strength≥ 450MPa
Yield Strength≥ 170MPa
Elongation≥ 30%
Elastic Modulus≥ 196GPa
Thermal Conductivity≥ 11.5W/m·K
thermal_expansion≥ 14.410⁻⁶/K
specific_heat≥ 460J/kg·K
max_use_temperature≥ 1100°C

Compatibility verdict

Alloy 800H / Incoloy 800H and N08810: null% composition match

Close equivalents but NOT identical.

Related materials

More Fe Ni Cr materials →

Not sure which material fits?

🤖 Ask AI Advisor →

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.