P265GH
1.0425Unalloyed pressure vessel steel — THE standard boiler plate material in Europe. ReH >=265 MPa, good weldability, guaranteed elevated-temperature properties to ~450°C. "GH" = suitable for use at elevated temperatures. Used for boilers, pressure vessels, heat exchangers, and steam drums per EN 10028-2 and PED 2014/68/EU.
International equivalents
| Flag | Standard | Country | Grade | Number | Match |
|---|---|---|---|---|---|
| 🇺🇸 | ASTM | USA | ASTM A516 Gr.60 (approximate) | — | REF |
| 🇪🇺 | EN | Europe | P265GH / 1.0425 | 1.0425 | 100% |
Sources: ASTM A516, EN 10028-2
Chemical composition comparison (wt%)
Side-by-side: P265GH (EN 10028-2) vs P265GH / 1.0425 (EN) (EN 10028-2)
| Element | P265GH (EN 10028-2) | P265GH / 1.0425 (EN) | Overlap |
|---|---|---|---|
| C | — | 0–0.2% | — |
| Si | — | 0–0.4% | — |
Mechanical properties
Compatibility verdict
P265GH and P265GH / 1.0425: 100% composition match
Related materials
C45
1.0503Medium carbon unalloyed quality steel. Good machinability and moderate strength after heat treatment. Widely used for shafts, spindles, pins, studs, and general machine parts.
S355JR
1.0045High-strength low-alloy structural steel with minimum yield strength of 355 MPa. Standard grade for bridges, buildings, cranes, and general structural applications. Impact tested at +20°C (JR).
S235JR
1.0038General-purpose structural steel with minimum yield strength of 235 MPa. The most common structural steel grade in Europe for general construction, frames, and non-critical structural applications.