Skip to content

X12CrNiMoV12-3

1.4422
Stainless SteelMartensitic
Compare with…Export PDF

Martensitic stainless for steam turbine blades and discs — 12Cr-3Ni-Mo-V. Higher Ni (2.5-3.5%) than X20Cr13 gives better toughness and corrosion resistance. V addition for creep strength at elevated temperatures. Used for LP/HP turbine blades, compressor discs, pump shafts, and valves in power generation. Service temperature to ~550°C.

International equivalents

FlagStandardCountryGradeNumberMatch
🇪🇺ENEuropeX12CrNiMoV12-3 / 1.44221.4422100%

Sources: EN 10088-3

Chemical composition comparison (wt%)

Side-by-side: X12CrNiMoV12-3 (EN) (EN 10088-3) vs X12CrNiMoV12-3 / 1.4422 (EN) (EN 10088-3)

ElementX12CrNiMoV12-3 (EN)X12CrNiMoV12-3 / 1.4422 (EN)Overlap
C0.08–0.15%0.08–0.15%OK
Mn0–1%0–1%OK
Cr11–12.5%11–12.5%OK
Mo1.5–2%1.5–2%OK
Ni2.5–3.5%2.5–3.5%OK
V0.25–0.35%0.25–0.35%OK

Mechanical properties

QT

PropertyValueUnit
Tensile Strength900–1100MPa
Yield Strength700–850MPa
Elongation12–16%
Elastic Modulus≥ 215GPa
Density≥ 7.7g/cm3

Compatibility verdict

X12CrNiMoV12-3 and X12CrNiMoV12-3 / 1.4422: 100% composition match

Close equivalents but NOT identical.

Related materials

More Martensitic materials →

Not sure which material fits?

🤖 Ask AI Advisor →

All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.