Skip to content

X2CrNiMoN25-7-4

1.4410
Stainless SteelDuplex
Compare with…Export PDF

Super duplex stainless steel (SAF 2507 / UNS S32750) with 25% Cr, 7% Ni, 4% Mo, and high N for PREN ≥42. The highest corrosion resistance and strength among standard duplex grades — YS ≥550 MPa is ~2.5× that of 316L. Service temperature up to 300°C. Used for subsea oil & gas equipment (manifolds, trees, risers), desalination plants, flue gas cleaning, chemical tankers, and mining equipment in severe chloride environments. Requires careful welding to avoid sigma phase.

Chemical composition comparison (wt%)

Side-by-side: X2CrNiMoN25-7-4 (EN) (EN 10088-2) vs ASTM

ElementX2CrNiMoN25-7-4 (EN)ASTMOverlap
C≤ 0.03%——
Si≤ 0.8%——
Mn≤ 1.2%——
P≤ 0.035%——
S≤ 0.015%——
Cr24–26%——
Mo3–5%——
Ni6–8%——
Cu≤ 0.5%——
N0.24–0.32%——

Mechanical properties

Solution Annealed

PropertyValueUnit
Tensile Strength800–1000MPa
Yield Strength≥ 550MPa
Elongation≥ 15%
Hardness HB≤ 310HB

General

PropertyValueUnit
Density≥ 7.8g/cm3

Related materials

More Duplex materials →

Not sure which material fits?