15-5PH / X5CrNiCuNb15-5 vs X17CrNi16-2: 37% composition overlap. Significantly different materials serving different application areas.
15-5PH / X5CrNiCuNb15-5 vs X17CrNi16-2
Side-by-side chemical composition and mechanical property comparison.
Overview
15-5PH / X5CrNiCuNb15-5
1.4545
Martensitic precipitation-hardening stainless steel. Similar to 17-4PH but with better transverse ductility and toughness due to lower delta ferrite. Used for aerospace structural components, nuclear reactor parts, food processing equipment, and high-performance fasteners.
X17CrNi16-2
1.4057
Martensitic CrNi stainless — AISI 431. Best corrosion resistance of ALL martensitic stainless steels due to high Cr (15-17%) + Ni (1.5-2.5%). Hardenable to HRC 46-50. Used for shafts, bolts, valve stems, pump components, fasteners in marine/offshore environments. Also aerospace (WL4044) and medical instruments. Service to 400°C.
| 15-5PH / X5CrNiCuNb15-5 | X17CrNi16-2 | |
|---|---|---|
| Material Number | 1.4545 | 1.4057 |
| Category | Stainless Steel | Stainless Steel |
| Standard | AMS 5659 | EN 10088-3 |
Chemical composition (wt%)
| Element | 15-5PH / X5CrNiCuNb15-5 | X17CrNi16-2 | Overlap |
|---|---|---|---|
| C | 0–0.07% | 0.12–0.22% | No overlap |
| Si | 0–1% | 0–1% | OK |
| Mn | 0–1% | 0–1.5% | OK |
| P | 0–0.03% | — | — |
Mechanical properties
| Property | 15-5PH / X5CrNiCuNb15-5 | X17CrNi16-2 | Unit |
|---|---|---|---|
| tensile_strength | ≥ 1310 | 800–950 | MPa |
| yield_strength | ≥ 1170 | ≥ 600 | MPa |
| elongation | ≥ 10 | ≥ 14 | % |
Compatibility Assessment
15-5PH / X5CrNiCuNb15-5 and X17CrNi16-2 have significantly different compositions (37% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is 15-5PH / X5CrNiCuNb15-5 the same as X17CrNi16-2?
15-5PH / X5CrNiCuNb15-5 and X17CrNi16-2 have a 37% composition overlap. They are generally not directly interchangeable.
Can I replace 15-5PH / X5CrNiCuNb15-5 with X17CrNi16-2?
Generally not recommended. The compositions differ significantly (37% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between 15-5PH / X5CrNiCuNb15-5 and X17CrNi16-2?
The main differences are in the following elements: C, Cr, Ni. 15-5PH / X5CrNiCuNb15-5 is a Stainless Steel grade, while X17CrNi16-2 is a Stainless Steel grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.