EN AW-5182 vs EN AW-6060: 48% composition overlap. Significantly different materials serving different application areas.
EN AW-5182 vs EN AW-6060
Side-by-side chemical composition and mechanical property comparison.
Overview
EN AW-5182
3.3519
One of the strongest non-heat-treatable Al-Mg alloys. 4.5% Mg + 0.35% Mn. THE standard alloy for beverage can lids/pull tabs (H48 temper). Also used for automotive body panels (hoods, doors), fuel tanks, and marine components. Excellent corrosion resistance and formability.
EN AW-6060
3.3206
The most extruded aluminum alloy in Europe — optimized for complex thin-walled extrusion profiles. Lower Mg+Si content than 6063/6082 provides excellent extrudability at moderate strength (UTS ~215 MPa T6). Good corrosion resistance, anodizability (decorative quality), and weldability. The default material for window/door frames, curtain wall mullions, railing systems, heat sinks, LED lighting profiles, and general architectural extrusions. EN AW-6063 is the closest ASTM equivalent.
| EN AW-5182 | EN AW-6060 | |
|---|---|---|
| Material Number | 3.3519 | 3.3206 |
| Category | Aluminum | Aluminum |
| Standard | EN 573-3 | EN 573-3 |
Chemical composition (wt%)
| Element | EN AW-5182 | EN AW-6060 | Overlap |
|---|---|---|---|
| Si | 0–0.2% | 0.3–0.6% | No overlap |
| Mn | 0.2–0.5% | ≤ 0.1% | No overlap |
| Cr | 0–0.1% | ≤ 0.05% | OK |
| Cu | 0–0.15% | ≤ 0.1% | OK |
Mechanical properties
| Property | EN AW-5182 | EN AW-6060 | Unit |
|---|---|---|---|
| tensile_strength | 275–330 | 190–230 | MPa |
| yield_strength | 130–190 | 150–190 | MPa |
| elongation | 20–25 | 8–14 | % |
Compatibility Assessment
EN AW-5182 and EN AW-6060 have significantly different compositions (48% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is EN AW-5182 the same as EN AW-6060?
EN AW-5182 and EN AW-6060 have a 48% composition overlap. They are generally not directly interchangeable.
Can I replace EN AW-5182 with EN AW-6060?
Generally not recommended. The compositions differ significantly (48% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between EN AW-5182 and EN AW-6060?
The main differences are in the following elements: Si, Mn, Mg. EN AW-5182 is a Aluminum grade, while EN AW-6060 is a Aluminum grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.