EN AW-5754 vs EN AW-6060: 43% composition overlap. Significantly different materials serving different application areas.

EN AW-5754 vs EN AW-6060

Side-by-side chemical composition and mechanical property comparison.

Overview

EN AW-5754

3.3535

Aluminum5xxx (Al-Mg)

Medium-strength non-heat-treatable aluminium alloy with good corrosion resistance and excellent weldability. Lower Mg than 5083 for better formability. The standard alloy for automotive body panels (inner), chemical equipment, and food industry applications.

EN AW-6060

3.3206

AluminumWrought

The most extruded aluminum alloy in Europe — optimized for complex thin-walled extrusion profiles. Lower Mg+Si content than 6063/6082 provides excellent extrudability at moderate strength (UTS ~215 MPa T6). Good corrosion resistance, anodizability (decorative quality), and weldability. The default material for window/door frames, curtain wall mullions, railing systems, heat sinks, LED lighting profiles, and general architectural extrusions. EN AW-6063 is the closest ASTM equivalent.

EN AW-5754EN AW-6060
Material Number3.35353.3206
CategoryAluminumAluminum
StandardEN 573-3EN 573-3

Chemical composition (wt%)

ElementEN AW-5754EN AW-6060Overlap
Si0–0.4%0.3–0.6%Partial
Mn0–0.5%≤ 0.1%OK
Cr0–0.3%≤ 0.05%OK
Cu0–0.1%≤ 0.1%OK

Mechanical properties

PropertyEN AW-5754EN AW-6060Unit
tensile_strength190–240190–230MPa
yield_strength≥ 80150–190MPa
elongation≥ 178–14%

Compatibility Assessment

EN AW-5754 and EN AW-6060 have significantly different compositions (43% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is EN AW-5754 the same as EN AW-6060?

EN AW-5754 and EN AW-6060 have a 43% composition overlap. They are generally not directly interchangeable.

Can I replace EN AW-5754 with EN AW-6060?

Generally not recommended. The compositions differ significantly (43% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between EN AW-5754 and EN AW-6060?

The main differences are in the following elements: Si, Mg. EN AW-5754 is a Aluminum grade, while EN AW-6060 is a Aluminum grade.

Related Comparisons

View full data for each material:

Data provided for reference only. Always verify against the applicable specification for critical applications.