Alloy 800H / Incoloy 800H vs Waspaloy: 31% composition overlap. Significantly different materials serving different application areas.
Alloy 800H / Incoloy 800H vs Waspaloy
Side-by-side chemical composition and mechanical property comparison.
Overview
Alloy 800H / Incoloy 800H
1.4958
Iron-nickel-chromium alloy (Fe-32Ni-21Cr) with controlled carbon (0.05–0.10%) and grain size for optimized creep-rupture strength above 600°C. Solution-annealed: Rm ≥450 MPa, Rp0.2 ≥170 MPa, A ≥30%. Density 7.94 g/cm³, E-Modul 196 GPa. Excellent resistance to carburization, oxidation, and nitriding to 1100°C. UNS N08810, ASTM B407/B408/B409. Applications: ethylene cracking tubes, reformer furnace tubes, heat exchangers, nuclear steam generators, chemical reactors. Variant 800HT (N08811/1.4959) has tighter Al+Ti control for even higher creep strength.
Waspaloy
2.4654
Nickel-based gamma-prime strengthened superalloy — THE turbine disc material. Excellent creep-rupture strength up to 650°C (rotating) and 870°C (static). Developed 1950s by Pratt & Whitney. Triple-aged (solution + stabilize + precipitation) for peak properties. Superior to Inconel 718 above 650°C. Used for compressor and rotor discs, shafts, spacers, seals, rings, casings, and fasteners in gas turbine engines.
| Alloy 800H / Incoloy 800H | Waspaloy | |
|---|---|---|
| Material Number | 1.4958 | 2.4654 |
| Category | Nickel Alloys | Nickel Alloys |
| Standard | EN 10302 / ASTM B407 | ASTM B637 |
Chemical composition (wt%)
| Element | Alloy 800H / Incoloy 800H | Waspaloy | Overlap |
|---|---|---|---|
| C | 0.05–0.1% | 0.02–0.1% | OK |
| Si | ≤ 1% | 0–0.75% | OK |
| Mn | ≤ 1.5% | 0–1% | OK |
| Cr | 19–23% | 18–21% | Partial |
Mechanical properties
| Property | Alloy 800H / Incoloy 800H | Waspaloy | Unit |
|---|---|---|---|
| density | ≥ 7.94 | ≥ 8.19 | g/cm3 |
| tensile_strength | ≥ 450 | 1170–1310 | MPa |
| yield_strength | ≥ 170 | 720–895 | MPa |
Compatibility Assessment
Alloy 800H / Incoloy 800H and Waspaloy have significantly different compositions (31% overlap). These materials are not interchangeable and serve different application areas.
Automated assessment based on composition analysis
Frequently Asked Questions
Is Alloy 800H / Incoloy 800H the same as Waspaloy?
Alloy 800H / Incoloy 800H and Waspaloy have a 31% composition overlap. They are generally not directly interchangeable.
Can I replace Alloy 800H / Incoloy 800H with Waspaloy?
Generally not recommended. The compositions differ significantly (31% overlap). These materials have different alloying concepts and are intended for different applications.
What is the difference between Alloy 800H / Incoloy 800H and Waspaloy?
The main differences are in the following elements: Cr, Al, Ti, Fe. Alloy 800H / Incoloy 800H is a Nickel Alloys grade, while Waspaloy is a Nickel Alloys grade.
Related Comparisons
View full data for each material:
Data provided for reference only. Always verify against the applicable specification for critical applications.
All data is for reference only. Equivalents indicate similarity, not identity. Always verify against the applicable specification for safety-critical applications. materialref.com accepts no liability for decisions based on this data.