Skip to content
Automated comparison · 0% overlap

FR-4 (Glass Epoxy Laminate) vs POM-C (Acetal Copolymer): 0% composition overlap. Significantly different materials serving different application areas.

FR-4 (Glass Epoxy Laminate) vs POM-C (Acetal Copolymer)

Side-by-side chemical composition and mechanical property comparison.

Sign up free for 3 comparisons per daySign up →

Overview

FR-4 (Glass Epoxy Laminate)

PolymersReinforced

Flame retardant woven fiberglass cloth with epoxy resin binder — the worldwide standard substrate material for printed circuit boards (PCBs). Designated NEMA grade FR-4 and IPC-4101. Good mechanical strength, dimensional stability and electrical insulation up to 130°C (Tg). Dielectric constant 4.2–4.7 at 1 MHz. Self-extinguishing (UL94 V-0). Used for single/multilayer PCBs, electrical insulation boards, structural composites in electronics, test fixtures and jigs. Available in thicknesses 0.1–50 mm.

POM-C (Acetal Copolymer)

PolymersEngineering

Polyoxymethylene Copolymer — the precision engineering plastic. Exceptional dimensional stability, low moisture absorption (0.2%), low friction coefficient, and excellent machinability. More hydrolysis-resistant and chemically stable than POM-H (homopolymer). No centerline porosity in stock shapes. Trade names include Hostaform (Celanese), Ertacetal C (MCAM), Duracon (Polyplastics). Used for gears, bearings, valve bodies, pump parts, electrical insulators, and food/medical contact parts.

FR-4 (Glass Epoxy Laminate)POM-C (Acetal Copolymer)
Material Number
CategoryPolymersPolymers
StandardIPC-4101ISO 10350

Chemical composition (wt%) — Pro

ElementFR-4 (Glass Epoxy Laminate)POM-C (Acetal Copolymer)Overlap
Epoxy Resin Matrix35–45%
Glass Fiber (E-Glass) Cloth55–65%
Polyoxymethylene (OCH2 units)95–99%
Ethylene Oxide Co-Monomer1–5%

Mechanical properties — Pro

PropertyFR-4 (Glass Epoxy Laminate)POM-C (Acetal Copolymer)Unit
Flexural Strength380–480MPa
Tensile Strength280–340MPa
Compressive Strength350–420MPa
Density
Glass Transition Temp (Tg)
Dielectric Constant (1MHz)
Dielectric Strength
UL94 Flammability
Water Absorption (24h)
Tensile Strength
Yield Strength
Elongation
Elastic Modulus
Density
Melting Point
Water Absorption (24h)
Continuous Use Temp

Sign up free and get 3 full comparisons immediately.

Sign up free — 3 comparisons/day free

Compatibility Assessment

FR-4 (Glass Epoxy Laminate) and POM-C (Acetal Copolymer) have significantly different compositions (0% overlap). These materials are not interchangeable and serve different application areas.

Automated assessment based on composition analysis

Frequently Asked Questions

Is FR-4 (Glass Epoxy Laminate) the same as POM-C (Acetal Copolymer)?

FR-4 (Glass Epoxy Laminate) and POM-C (Acetal Copolymer) have a 0% composition overlap. They are generally not directly interchangeable.

Can I replace FR-4 (Glass Epoxy Laminate) with POM-C (Acetal Copolymer)?

Generally not recommended. The compositions differ significantly (0% overlap). These materials have different alloying concepts and are intended for different applications.

What is the difference between FR-4 (Glass Epoxy Laminate) and POM-C (Acetal Copolymer)?

The main differences are in the following elements: overall alloying content. FR-4 (Glass Epoxy Laminate) is a Polymers grade, while POM-C (Acetal Copolymer) is a Polymers grade.